Polymer Property : Flexural Modulus, 1% Secant = 769 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 5.30 MPa
769 psi
ASTM D790 and ISO 178
ExxonMobil Exact™ 9361 Ethylene-based Plastomer Resin
Product Description: Exact 9361 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:P..