Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 520 MPa | 75400 psi | ASTM-D790 |
Braskem RD34U3 LLDPE Rotomolding Polyethylene The resin RD34U3 is a linear low-density polyethylene, 1-butene based, with excellent processability and a good balance of stiffness and impact strength. It contains long term UV6 stabilization and .. |
|||
Flexural Modulus, 1% Secant | 520 MPa | 75400 psi | ASTM-D790 |