Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 580 MPa
84100 psi
ASTM D 790
NOVA Chemicals Surpass® IFs932-R Octene SLLDPE Injection Molding Resin
IFs932-R complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem..