Polymer Property : Flexural Modulus, 1% Secant = 53700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 370 MPa
53700 psi
ASTM-D790
Braskem IC32 LLDPE Injection Molding Polyethylene Copolymer
IC32 is a linear low-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding. It offers good fluidity, excellent flexibility and tenac..