Polymer Property : Flexural Modulus, 1% Secant = 41000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 283 MPa
41000 psi
ASTM D790
ExxonMobil LDPE LD 637.LI Low Density Polyethylene Resin
Product Description: LD 637.LI is a high melt index LDPE homopolymer intended for injection molding or compounding applications requiring high flow. It is ideal for tamper-evident, tear-to-open clos..
Flexural Modulus, 1% Secant 283 MPa
41000 psi
ASTM D790
ExxonMobil LLDPE LL 6201RQ Molding Linear Low Density Polyethylene Resin (European Grade)
Product Description: LL 6201 series are high flow LLDPE grades, which offer unique combination of excellent processability and outstanding product properties. Parts manufactured from LL 6201 Have go..
Flexural Modulus, 1% Secant 283 MPa
41000 psi
ASTM D790
ExxonMobil LLDPE LL 6201XR Molding Linear Low Density Polyethylene Resin (European Grade)
Product Description: LL 6201 series are high flow LLDPE grades, which offer unique combination of excellent processability and outstanding product properties. Parts manufactured from LL 6201 Have go..