Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 276 MPa
40000 psi
ASTM D638
ExxonMobil LLDPE LL 5002.09 Linear Low Density Polyethylene Resin
Product Description: LL 5002.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. LL 5002.09 also exhibits good toughness and environmental str..