Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 214 MPa
31000 psi
ASTM D790
ExxonMobil LDPE LD 101BA Wire & Cable Low Density Polyethylene Resin
Product Description: LD 101BA Wire & Cable is anon-stabilized LDPE, designed for the production of Medium/High Voltage insulation using the direct peroxide addition. For cleanliness reasons, the mat..
Flexural Modulus, 1% Secant 214 MPa
31000 psi
ASTM D790
ExxonMobil LDPE LD 503.LP Low Density Polyethylene Resin
Product Description: LD 503.LP is a LDPE homopolymer that is suitable for use in molding, extrusion, compounding and foam applications.Availability: Latin America, North America and South AmericaAdd..