Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 3003 MPa | 435500 psi | ASTM D-790A |
Bapolan® 6055 Polystyrene, Injection Molding Bapolan PS6055 is a crystal polystyrene resin designed for injection molding applications requiring fast cycle times and superior optical properties. It complies with US FDA21 CFR177.1640 and 94HB .. |