Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus, 1% Secant = 280100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 1931 MPa
280100 psi
ASTM D790
Entec Hypro™ PP-HP20NS Homopolymer, 20 Melt Flow, Nucleated, Anti-stat
This product is intended for general purpose injection molding applications such as cutlery, caps and closures, and thin-wall containers.Information provided by Entec
Copyright © lookpolymers.com All Rights Reserved