Polymer Property : Flexural Modulus, 1% Secant = 276000 psi
Polymer Property :
Flexural Modulus, 1% Secant =
276000 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Modulus, 1% Secant
1900
MPa
276000
psi
ASTM D790A
Braskem H 501HC Thermoforming Polypropylene Homopolymer
High-stiffness thermoformed parts.Information provided by Braskem.