Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 1860 MPa
270000 psi
ASTM D790B
ExxonMobil HDPE HD 6909.19 High Density Polyethylene Copolymer Resin
Product Description: HD 6908 is a homopolymer with outstanding stiffness with a good balance of processability and cold temperature impact performance. This resin is ideally suited for articles requ..
Flexural Modulus, 1% Secant 1860 MPa
270000 psi
ASTM D790B
ExxonMobil HDPE HD 6909.65 High Density Polyethylene Copolymer Resin
Product Description: HD 6908 is a homopolymer with outstanding stiffness with a good balance of processability and cold temperature impact performance. This resin is ideally suited for articles requ..