Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 1725 MPa
250200 psi
ASTM D790
Entec Hypro™ PP-HP35NS Homopolymer, 35 Melt Flow, Nucleated, Anti-stat
This product is intended for thin-wall injection molding applications such as caps and closures, food containers and consumer products that require high stiffness.Information provided by Entec