Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus, 1% Secant = 215100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 1483 MPa
215100 psi
ASTM D790
Flint Hills P4G2Z-159 Polypropylene Homopolymer
Features: High xylene soluble. Product does not contain animal derived components. Phthalate-free.Applications: Extrusion: BOPP FilmInformation Provided by Flint Hills Resources