Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 212 MPa | 30700 psi | ASTM D-790 |
Bapolene® 213B Polyethylene, Extrusion Grade Bapolene 213B is a low density polyethylene for molding, extrusion and foaming applications. It contains slip and complies with US FDA regulation 21 CFR 177.1520 (Olefin polymers), paragraph (c)2.1.. |