Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 1320 MPa
191000 psi
ASTM-D790
Braskem GM8250T HDPE High Density Extrusion Polyethylene
GM8250T is a high-density polyethylene specially developed for the manufacturing of corrugated pipes. It has high molar mass and shows excellent tenacity, high stiffness, good impact resistance, and..
Copyright © lookpolymers.com All Rights Reserved