Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1230 MPa | 179000 psi | 0.05 in/min; ASTM D790A |
ExxonMobil PP7654KNE2 Polypropylene Homopolymer Product Description: A high impact copolymer resin with medium melt flow rate and excellent processing attributes. It is designed for injection molded large consumer and industrial parts.Availabili.. |