Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 1200 MPa
174000 psi
ASTM D790A
SABIC PP 513MN40 Polypropylene Impact Copolymer for Injection Molding
Product Description: PP 513MN40 is a controlled rheology PP grade of narrow molecular weight distribution. It contains an antistatic agent and is especially developed for producing injection molde..
Flexural Modulus, 1% Secant 1200 MPa
174000 psi
ASTM D790
Flint Hills P9M7R-056 Specialty Homopolymer Polypropylene
Clarified, e-beam and Gamma radiation sterilizable and Autoclavable. Product does not contain animal derived components. Phthalate-free.Applications: Injection molding - Lab ware, Pipette tips.In..
Flexural Modulus, 1% Secant 1200 MPa
174000 psi
ASTM-D790
Braskem GP5550BK HDPE High Density Extrusion Polyethylene
GP5550BK is a high-density polyethylene with high molar mass. It is produced with bimodal technology and shows excellent mechanical properties and high resistance to stress cracking. GP5550BK contai..
Flexural Modulus, 1% Secant 1200 MPa
174000 psi
ASTM-D790
Braskem IA58 HDPE Injection Molding Polyethylene Copolymer
IA58 is a high-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers good processability combined with good ..
Flexural Modulus, 1% Secant 1200 MPa
174000 psi
ASTM-D790
Braskem IA59U3 HDPE Injection Molding Polyethylene Homopolymer
IA59U3 is a high-density polyethylene, narrow molecular weight homopolymer produced by the solution process for injection molding applications. It offers high stiffness and impact strength combined ..
Flexural Modulus, 1% Secant 1200 MPa
174000 psi
ASTM-D790
Braskem PH 0952 HOMO Polypropylene Homopolymer
PH 0952 is a medium melt flow rate homopolymer with slip and antiblocking agents. This product is designed for technical films and packaging for cast and blown film extrusion. This product features ..
Flexural Modulus, 1% Secant 1200 MPa
174000 psi
ASTM D790A
Braskem H 103 Extrusion Coating Polypropylene Homopolymer
Description: H 103 is a high melt flow rate additivated homopolymer used for general purposes. The product exhibits excellent processing performance on injection moulding applications. Applications:..
Flexural Modulus, 1% Secant 1200 MPa
174000 psi
ASTM-D790
Braskem IE59U3 HDPE Injection Molding Polyethylene Homopolymer
IE59U3 is a high-density polyethylene, narrow molecular weight homopolymer produced by the solution process for injection molding applications. It offers high stiffness and impact strength, good pro..