Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1655 MPa | 240000 psi | ASTM D790 |
Entec Hypro™ PP-HP12 Homopolymer, 12 Melt Flow This product in intended for general purpose injection molding applications such as caps and closures, resin furniture and consumer products.Information provided by Entec |
|||
Flexural Modulus, 1% Secant | 1655 MPa | 240000 psi | ASTM D790 |