Flexural Modulus, 1% Secant 890 MPa
129000 psi
ASTM-D790
Braskem GM7746C HDPE Blow Molding Polyethylene
GM7746C is a high-density polyethylene specially developed for the manufacturing of blow molding fuel tanks. It has high molar mass and excellent mechanical properties. It also shows excellent tenac..
Flexural Modulus, 1% Secant 890 MPa
129000 psi
ASTM-D790
Braskem GM7746CA HDPE Blow Molding Polyethylene
GM7746CA is a high-density polyethylene specially developed for the manufacturing of blow molding fuel tanks. It has high molar mass and excellent mechanical properties. It also shows excellent tena..