Polymer Property : Flexural Modulus, 1% Secant = 1190 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 1190 MPa
172000 psi
0.05 in/min; ASTM D790A
ExxonMobil PP5341E1 Polypropylene Homopolymer
Product Description: A low melt flow rate that provides high melt strength and resistance to softening at elevated temperature.Availability: North America Features:Low FlowUses: Automotive Applic..
Flexural Modulus, 1% Secant 1190 MPa
173000 psi
0.05 in/min; ASTM D790A
ExxonMobil PP8255E1 Polypropylene Homopolymer
Product Description: A high crystallinity, medium impact copolymer resin designed for compounded and injection molded applications requiring high melt flow rate and excellent processing attributes...
Flexural Modulus, 1% Secant 1190 MPa
173000 psi
ASTM-D790
Braskem IG58 HDPE Injection Molding Polyethylene Copolymer
IG58 is a high-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers high stiffness, impact strength and out..