Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1175 MPa | 170400 psi | ASTM D790 |
Entec Hypro™ PP-CP35/2 Impact Copolymer, 35 Melt Flow This product is intended for general purpose injection molding applications including consumer products, housewares and packaging.Information provided by Entec |