Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 1160 MPa
168000 psi
ASTM D790
Entec Hypro™ PP-CP20/2 Impact Copolymer, 20 Melt Flow
This product is intended for general purpose injection molding applications including automotive and consumer products, large buckets and pails where toughness and cold temperature impact are requir..
Flexural Modulus, 1% Secant 1160 MPa
168000 psi
ASTM-D790
Braskem GM8260 HDPE Blow Molding Polyethylene Homopolymer
HDPE GM8260 is a high-density polyethylene homopolymer that has high molecular weight and was developed for the blow molding segment of large volumes. Its applications include: drums for lubricant ..