Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 110 MPa | 16000 psi | ASTM D790 |
ExxonMobil Vistamaxx™ 3980FL Propylene-based Elastomer - High Purity, Low Gel Product Description: Vistamaxx 3980FL propylene-based elastomer is an olefinic elastomer primarily composed of isostatic propylene repeat units with random ethylene distribution. It is produced us.. |