Polymer Property : Flexural Modulus, 1% Secant = 104000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 720 MPa
104000 psi
ASTM D790
Flint Hills P6E2A-005B Polypropylene Impact Copolymer
Features: Ultra high impact strength and long term heat aging.Applications: Injection molding and extrusion: high pressure resistance, film and flexible profilesInformation Provided by Flint Hills R..