Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 689 MPa | 100000 psi | ASTM D638 |
ExxonMobil LLDPE LL 8555.24 Linear Low Density Polyethylene Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Flexural Modulus, 1% Secant | 689 MPa | 100000 psi | ASTM D638 |
ExxonMobil LLDPE LL 8555.25 Linear Low Density Polyethylene Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Flexural Modulus, 1% Secant | 689 MPa | 100000 psi | ASTM D638 |
ExxonMobil LLDPE LLP 8555.24 Linear Low Density Polyethylene Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Flexural Modulus, 1% Secant | 689 MPa | 100000 psi | ASTM D638 |
ExxonMobil LLDPE LLP 8555.25 Linear Low Density Polyethylene Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |