Mechanical Properties Metric English Comments
Tear Strength 47.0 kN/m

@Thickness 2.00 mm,
Temperature 23.0 °C
268 pli

@Thickness 0.0787 in,
Temperature 73.4 °F
Method A, Trouser; Flow; ISO 34-1
PolyOne OnFlex™ BIO 5370A-E0004 Thermoplastic Elastomer (TPE)
OnFlex™-Bio 5300 series thermoplastic elastomer compounds are soft thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% of renewable materi..
Tear Strength 47.0 kN/m

@Thickness 2.00 mm,
Temperature 23.0 °C
268 pli

@Thickness 0.0787 in,
Temperature 73.4 °F
Method A, Trouser, 500 mm/min Across Flow; ISO 34-1
PolyOne OnFlex™ U 5370A-E0077 Thermoplastic Elastomer (TPE)
OnFlex™ U thermoplastic elastomer compounds are based on thermoplastic polyurethane elastomers (TPE-U). The OnFlex™ U 5300 series are based upon alloys of SEBS and TPU, combining the advantages of..