Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 56.0 kN/m @Thickness 2.00 mm, Temperature 23.0 °C |
320 pli @Thickness 0.0787 in, Temperature 73.4 °F |
Method A, Trouser, 500 mm/min Across Flow; ISO 34-1 |
PolyOne OnFlex™ U 5470A-E0083 Thermoplastic Elastomer (TPE) OnFlex™-U thermoplastic elastomer compounds are based on thermoplastic polyurethane elastomers (TPE-U). The OnFlex™-U 5400 series are based upon alloys of SEBS and aliphatic TPU, combining the adv.. |