Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 0.330 kN/m @Time 1190 sec |
1.88 pli @Time 0.330 hour |
Peel Adhesion, 180° Peel, to ABS; ASTM D1000 |
Rogers Corporation Poron® 4790-79SP-15012 Urethane Shock Pad Foam Information provided by Rogers Corporation. |
|||
Tear Strength | 0.330 kN/m @Time 1190 sec |
1.88 pli @Time 0.330 hour |
Peel Adhesion, 180° Peel, to Acrylic; ASTM D1000 |
Rogers Corporation Poron® 4790-79SP-15012 Urethane Shock Pad Foam Information provided by Rogers Corporation. |
|||
Tear Strength | 0.330 kN/m @Time 1190 sec |
1.88 pli @Time 0.330 hour |
Peel Adhesion, 180° Peel, to ABS; ASTM D1000 |
Rogers Corporation Poron® ThinStik ShockSeal™ 79-09021 Self-Adhesive Urethane Foam PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits.. |
|||
Tear Strength | 0.330 kN/m @Time 1190 sec |
1.88 pli @Time 0.330 hour |
Peel Adhesion, 180° Peel, to Acrylic; ASTM D1000 |
Rogers Corporation Poron® ThinStik ShockSeal™ 79-09021 Self-Adhesive Urethane Foam PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits.. |
|||
Tear Strength | 0.330 kN/m @Time 1190 sec |
1.88 pli @Time 0.330 hour |
Peel Adhesion, 180° Peel, to ABS; ASTM D1000 |
Rogers Corporation Poron® ThinStik Soft Seal 15-06021 Self-Adhesive Urethane Foam PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits.. |
|||
Tear Strength | 0.330 kN/m @Time 1190 sec |
1.88 pli @Time 0.330 hour |
Peel Adhesion, 180° Peel, to Acrylic; ASTM D1000 |
Rogers Corporation Poron® ThinStik Soft Seal 15-06021 Self-Adhesive Urethane Foam PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits.. |
|||
Tear Strength | 0.330 kN/m @Time 1190 sec |
1.88 pli @Time 0.330 hour |
Peel Adhesion, 180° Peel, to ABS; ASTM D1000 |
Rogers Corporation Poron® ThinStik Soft Seal 15-06030 Self-Adhesive Urethane Foam PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits.. |
|||
Tear Strength | 0.330 kN/m @Time 1190 sec |
1.88 pli @Time 0.330 hour |
Peel Adhesion, 180° Peel, to Acrylic; ASTM D1000 |
Rogers Corporation Poron® ThinStik Soft Seal 15-06030 Self-Adhesive Urethane Foam PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits.. |
|||
Tear Strength | 0.330 kN/m @Time 1190 sec |
1.88 pli @Time 0.330 hour |
Peel Adhesion, 180° Peel, to ABS; ASTM D1000 |
Rogers Corporation Poron® ThinStik™ 92-09020 Self-Adhesive Urethane Foam PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits.. |
|||
Tear Strength | 0.330 kN/m @Time 1190 sec |
1.88 pli @Time 0.330 hour |
Peel Adhesion, 180° Peel, to Acrylic; ASTM D1000 |
Rogers Corporation Poron® ThinStik™ 92-09020 Self-Adhesive Urethane Foam PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits.. |
|||
Tear Strength | 0.330 kN/m @Time 1190 sec |
1.88 pli @Time 0.330 hour |
Peel Adhesion, 180° Peel, to ABS; ASTM D1000 |
Rogers Corporation Poron® ThinStik™ 92-12020 Self-Adhesive Urethane Foam PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits.. |
|||
Tear Strength | 0.330 kN/m @Time 1190 sec |
1.88 pli @Time 0.330 hour |
Peel Adhesion, 180° Peel, to Acrylic; ASTM D1000 |
Rogers Corporation Poron® ThinStik™ 92-12020 Self-Adhesive Urethane Foam PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits.. |