Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 5.00 MPa @Temperature 120 °C |
725 psi @Temperature 248 °F |
|
LATI Lastilac 11 G/10 ABS/PC, 10% Glass Fiber Reinforced ABS/PC Blend (ABS/PC) based compound. Glass fibers. Good surface appearance. Good impact resistance. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; .. |
|||
Tensile Strength at Break | 5.00 MPa @Temperature 90.0 °C |
725 psi @Temperature 194 °F |
|
LATI Latene® AG9H MI/40 PP Homopolymer, 40% Mica Reinforced, Heat Stabilized Polypropylene homopolymer (PPh) based compound. Chemical grafting Heat stabilized. Mica filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provi.. |