Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 4.81 MPa @Temperature 23.0 °C |
698 psi @Temperature 73.4 °F |
Die C Flow 2 hr; ASTM D412 |
PolyOne Versalloy™ HC 9220-70 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-70 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |