Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 422 MPa @Temperature 100 °C |
>= 61200 psi @Temperature 212 °F |
|
PEAK Werkstoff DISPAL S542 Aluminum Alloy, AlMg6Mn4SiTiZrCo, Condition F Information provided by PEAK Werkstoff GmbH |