Mechanical Properties Metric English Comments
Tensile Strength at Break >= 414 MPa

@Thickness <=25.4 mm
>= 60000 psi

@Thickness <=1.00 in
Cadi 150 Copper Alloy
A small addition of Zr to copper improves resistance to softening and resists deformation at high temperatures where normal copper would soften rapidly. Zirconium copper is used as a Class 1 electr..
Tensile Strength at Break >= 414 MPa

@Thickness <=25.4 mm
>= 60000 psi

@Thickness <=1.00 in
Cadi 162 Copper Alloy
Cadmium addition to copper increases hardness and resistance to softening. C16200 is utilized in numerous applications where fatigue strength and high electrical conductivity are required. Cadmium..