Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 411 MPa @Temperature 150 °C |
>= 59600 psi @Temperature 302 °F |
|
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6x Heat Treatment Condition T6x (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials all.. |
|||
Tensile Strength at Break | >= 411 MPa @Temperature 100 °C |
>= 59600 psi @Temperature 212 °F |
|
PEAK Werkstoff DISPAL S541 Aluminum Alloy, AlMg6Mn4SiTiZr, Condition F Information provided by PEAK Werkstoff GmbH |