Mechanical Properties Metric English Comments
Tensile Strength at Break >= 410 MPa

@Thickness 3.00 mm
>= 59500 psi

@Thickness 0.118 in
ThyssenKrupp COR-TEN A Structural Steel
This Material Specification applies to plates up to 12.5 mm in thickness made from COR-TEN A.Definition: Weathering means that due to its chemical composition the COR-TEN A steel, when utilized unpr..