Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 350 MPa @Temperature 950 °C |
50800 psi @Temperature 1740 °F |
|
Special Metals UDIMET® alloy 520 Superalloy UDIMET® alloy 520 is a precipitation-hardenable nickel base superalloy with an exceptional combination of high-temperature mechanical properties, corrosion resistance and forgeability characteris.. |