Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 310 MPa @Thickness >=63.5 mm |
45000 psi @Thickness >=2.50 in |
|
Carlson 70 30 Cu Ni Copper-Nickel Alloy General DescriptionCarlson alloy 70 30 Cu Ni is a copper nickel alloy with excellent resistance to corrosion and erosion. It is strong and ductile. 70 30 Cu Ni is utilized in areas where high temp.. |