Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 448 MPa @Temperature 20.0 °C |
>= 65000 psi @Temperature 68.0 °F |
|
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition T6 Heat Treatment Condition T6 (Quenching in water at RT)Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo.. |