Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 400 MPa @Temperature 700 °C |
58000 psi @Temperature 1290 °F |
R<sub>m</sub> |
Assab Steels HOTVAR Hot Work Steel HOTVAR is a high performance molybdenum-vanadium alloyed hot-work tool steel which is characterized by:High hot wear resistanceVery good high temperature propertiesHigh resistance to thermal fatigue.. |