Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 38.0 MPa @Temperature 120 °C |
5510 psi @Temperature 248 °F |
ASTM Test |
BASF Ultramid® SEGM35 H1 BK-126 15/25% Glass/Mineral Filled PA6 (Conditioned) Ultramid SEGM35 H1 BK-126 is a 40% glass/mineral reinforced injection molding grade. It offers enhanced surface appearance, it also exhibits similar UV weathering characteristics compared to 8267G .. |
|||
Tensile Strength at Break | 38.0 MPa @Temperature 120 °C |
5510 psi @Temperature 248 °F |
ISO Data |
BASF Ultramid® SEGM35 H1 BK-126 15/25% Glass/Mineral Filled PA6 (Conditioned) Ultramid SEGM35 H1 BK-126 is a 40% glass/mineral reinforced injection molding grade. It offers enhanced surface appearance, it also exhibits similar UV weathering characteristics compared to 8267G .. |