Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 255 MPa @Temperature 23.0 °C |
37000 psi @Temperature 73.4 °F |
|
LATI Larpeek 10 K/40 PEEK, 40% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |