Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 245 MPa @Temperature 23.0 °C |
35500 psi @Temperature 73.4 °F |
|
LATI Laramid G/45 PPA, 45% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Tensile Strength at Break | 245 MPa @Temperature 90.0 °C |
35500 psi @Temperature 194 °F |
|
LATI Laramid K/40 HM PPA, 40% Carbon Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Carbon fiber. High tensile modulus. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; .. |