Polymer Property : Tensile Strength at Break = 345 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 345 MPa

@Thickness >=25.4 mm
>= 50000 psi

@Thickness >=1.00 in
Cadi 150 Copper Alloy
A small addition of Zr to copper improves resistance to softening and resists deformation at high temperatures where normal copper would soften rapidly. Zirconium copper is used as a Class 1 electr..
Tensile Strength at Break >= 345 MPa

@Thickness >=25.4 mm
>= 50000 psi

@Thickness >=1.00 in
Cadi 162 Copper Alloy
Cadmium addition to copper increases hardness and resistance to softening. C16200 is utilized in numerous applications where fatigue strength and high electrical conductivity are required. Cadmium..
Tensile Strength at Break >= 345 MPa

@Thickness <=63.5 mm
>= 50000 psi

@Thickness <=2.50 in
Carlson 70 30 Cu Ni Copper-Nickel Alloy
General DescriptionCarlson alloy 70 30 Cu Ni is a copper nickel alloy with excellent resistance to corrosion and erosion. It is strong and ductile. 70 30 Cu Ni is utilized in areas where high temp..