Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 23.5 MPa @Temperature 145 °C, Time 2990 sec |
3410 psi @Temperature 293 °F, Time 0.830 hour |
cured; ASTM D412 |
LG Chemical NBR 7030 High Acrylonitrile Polymer Description: NBR 7030 is a mechanically fully-fluxed polyblend of 70 parts medium-high acrylonitrile rubber and 30 parts polyvinylchloride resin. Since NBR 7030 are prefluxed, normal temperature for.. |