Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 33.7 MPa @Temperature 145 °C, Time 2990 sec |
4890 psi @Temperature 293 °F, Time 0.830 hour |
cured; ASTM D412 |
LG Chemical NBR 3280 High Acrylonitrile Polymer Description: NBR 3280 is a copolymer of butadiene and acrylonitrile manufactured by cold emulsion polymerization technology of Goodyear Tire and Rubber Company, USA. NBR 3280 is a non staining, high.. |