Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 21.5 MPa @Temperature 100 °C, Time 259000 sec |
3120 psi @Temperature 212 °F, Time 72.0 hour |
Circulating Oven Aging |
LG Chemical NBR 6280 High Acrylonitrile Polymer Description: NBR 6280 is a copolymer of butadiene and acrylonitrile manufactured by advanced emulsion polymerization technology of Goodyear and LG Chem. NBR 6280 is a non staining, high mooney, and .. |