Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 30.1 MPa @Temperature 145 °C, Time 2990 sec |
4370 psi @Temperature 293 °F, Time 0.830 hour |
cured; ASTM D412 |
LG Chemical NBR 6280 High Acrylonitrile Polymer Description: NBR 6280 is a copolymer of butadiene and acrylonitrile manufactured by advanced emulsion polymerization technology of Goodyear and LG Chem. NBR 6280 is a non staining, high mooney, and .. |