Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 3.38 MPa @Temperature 121 °C, Time 605000 sec |
490 psi @Temperature 250 °F, Time 168 hour |
JRF; AMS-S83318 |
3M AC-250 B-1/6 Aerospace Sealant 3M Aerospace Sealant AC-250 B-1/6 is a two-part, polysulfide, quick repair sealant for integral fuel tank and fuselage sealing applications. The mixed compound is a thixotropic paste and can be read.. |