Tensile Strength at Break 260 MPa

@Temperature 23.0 °C
37700 psi

@Temperature 73.4 °F
LATI Laramid G/50 PPA, 50% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Tensile Strength at Break 260 MPa

@Temperature 23.0 °C
37700 psi

@Temperature 73.4 °F
Dry; EN2561
Hexcel® HexTOOL™ M61 Quasi-isotropic High Temperature Prepreg Tooling Compound
HexTOOL™ Tooling Compound is randomly layered strips of uni-directional prepreg which is consolidated into rolled goods. It can be utilized as multi-ply quasi-isotropic hand lay-up, and subsequentl..