Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 249 MPa @Temperature -40.0 °C |
36100 psi @Temperature -40.0 °F |
ISO 527 |
BASF Ultramid® KR 4357 G6 30% Glass Filled PA6/6T (Dry) Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan.. |