Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 14.5 MPa @Temperature 23.0 °C |
2100 psi @Temperature 73.4 °F |
ASTM D1708 |
Solvay Specialty Polymers Hyflon® PFA P220 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resis.. |